Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3K FC Aqua UN - PA66 - BASF

Material Data Center offers the following functions for Ultramid® A3K FC Aqua UN:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Ultramid® A3K FC Aqua UN is optimized for plastic parts, mandatory requiring material approvals for drinking water or direct food contact.

The product is approved according to
• 21 CFR FDA § 177.1500 "Nylon resins" (except contact with alcoholic beverages)
• European Food Contact European Food Contact Commission Regulation (EU) 10/2011
• GMP (EC) n°2023/2006

and provides the approvals for drinking water regulations of
• KTW
• DVGW W270
• WRAS
• ACS (disclosure of ingredients)
• NSF (disclosure of ingredients)

For questions regarding the compliance with further regulations, and certificates, please contact your local BASF representative or Plastics Safety (E-Mail: plastics.safety@basf.com).
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 115 / * cm³/10min ISO 1133
온도 275 / * °C -
하중 5 / * kg -
성형 수축률, 평행 1.6 / * % ISO 294-4, 2577
성형 수축률, 수직 1.8 / * % ISO 294-4, 2577
이형온도 180 °C -
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 3100 / 1100 MPa ISO 527
항복강도 85 / 50 MPa ISO 527
항복변형률 5 / 20 % ISO 527
파단시 평균신율 30 / >50 % ISO 527
굴곡 계수, 23°C 2900 / - MPa ISO 178
탄성변형률, 1h * / 1100 MPa ISO 899-1
탄성변형률, 1000h * / 700 MPa ISO 899-1
챠피 충격 강도 , +23°C N / N kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C N / - kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 5 / 20 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 4 / - kJ/m² ISO 179/1eA
아이조드 충격은 노치, +23°C 5.5 / N kJ/m² ISO 180/1A
아이조드 충격은 노치 6 / - kJ/m² ISO 180/1A
온도 -30 °C -
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 260 / * °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min 72 / * °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 75 / * °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 220 / * °C ISO 75-1/-2
비카트 연화 온도, B 250 / * °C ISO 306
선형 열팽창 계수, 평행 98 / * E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 V-2 / * class IEC 60695-11-10
테스트 두께 1.6 / * mm -
산소지수로서의 난연성 28 / * % ISO 4589-1/-2
전기적 특성건조/응축단위시험규격
ISO 데이터
상대 유전율, 100Hz 3.8 / - - IEC 62631-2-1
상대 유전뮬, 1MHz 3.2 / 5 - IEC 62631-2-1
소산 인자, 100Hz 50 / - E-4 IEC 62631-2-1
소산 인자, 1MHz 250 / 2000 E-4 IEC 62631-2-1
부피 저항 1E13 / 1E10 Ohm*m IEC 62631-3-1
표면 저항 * / 1E10 Ohm IEC 62631-3-2
CTI - / 600 - IEC 60112
기타 특성건조/응축단위시험규격
물에서의 흡수성 8.5 / * % ISO 62와 유사
조건에서의 흡습성 2.8 / * % ISO 62와 유사
밀도 1130 / - kg/m³ ISO 1183
Bulk density 700 kg/m³ -
물질의 비성질건조/응축단위시험규격
ISO 데이터
점도수 150 / * cm³/g ISO 307, 1157, 1628
테스트 견본 생산단위시험규격
ISO 데이터
사출성형: 용융수지온도 290 °C ISO 294
사출성형: 금형온도 80 °C ISO 294
사출성형: 사출속도 200 mm/s ISO 294
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.15 % -
용융수지온도 280 - 300 °C -
성형온도 60 - 80 °C -
도표
점도-변형률 , Ultramid® A3K FC Aqua UN, PA66, BASF
전단-변형률 , Ultramid® A3K FC Aqua UN, PA66, BASF
동전단탄성율-온도 , Ultramid® A3K FC Aqua UN (건조), PA66, BASF
동전단탄성율-온도 , Ultramid® A3K FC Aqua UN (응축), PA66, BASF
응력-신율 , Ultramid® A3K FC Aqua UN (건조), PA66, BASF
응력-신율 , Ultramid® A3K FC Aqua UN (응축), PA66, BASF
시컨트탄성율-신율 , Ultramid® A3K FC Aqua UN (건조), PA66, BASF
시컨트탄성율-신율 , Ultramid® A3K FC Aqua UN (응축), PA66, BASF
응력-신율(등시) 23°C, Ultramid® A3K FC Aqua UN (응축), PA66, BASF
크립탄성율-시간 23°C, Ultramid® A3K FC Aqua UN (응축), PA66, BASF
곡선 크리프 23°C, Ultramid® A3K FC Aqua UN (응축), PA66, BASF
응력-신율(등시) 60°C, Ultramid® A3K FC Aqua UN (건조), PA66, BASF
크립탄성율-시간 60°C, Ultramid® A3K FC Aqua UN (건조), PA66, BASF
곡선 크리프 60°C, Ultramid® A3K FC Aqua UN (건조), PA66, BASF
응력-신율(등시) 90°C, Ultramid® A3K FC Aqua UN (건조), PA66, BASF
크립탄성율 -시간 90°C, Ultramid® A3K FC Aqua UN (건조), PA66, BASF
곡선 크리프 90°C, Ultramid® A3K FC Aqua UN (건조), PA66, BASF
응력-신율(등시) 120°C, Ultramid® A3K FC Aqua UN (건조), PA66, BASF
크립탄성율-시간 120°C, Ultramid® A3K FC Aqua UN (건조), PA66, BASF
곡선 크리프 120°C, Ultramid® A3K FC Aqua UN (건조), PA66, BASF
비용적-온도(pvT) , Ultramid® A3K FC Aqua UN, PA66, BASF
인장탄성율-온도 , Ultramid® A3K FC Aqua UN (건조), PA66, BASF
인장탄성율-온도 , Ultramid® A3K FC Aqua UN (응축), PA66, BASF
특징
생산 공정
사출 성형, 기타 압출
인도 유형
펠렛 (입자,알갱이), 자연 색상
부가물
윤활제, 이형제
특별 특성
열안정성
Certifications
Food contact, Food approval 10/2011, Food approval FDA 21 CFR, Drinking water contact, Drinking water contact KTW, Drinking water contact DVGW W270, Drinking water contact NSF 61
응용
자동차의
지역별 검색
기타 정보
사E성
PREPROCESSING
Pre/Post-processing, max. allowed water content: .15 %
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 280 - 300 °C
injection molding, Melt temperature, recommended: 290 °C
injection molding, Mold temperature, range: 60 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
injection molding, Dwell time, thermoplastics: 10 min
화학적 매체에 대한 저항력
에서의 아세트산 (질량 5%) (23°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.